Magnetic Stripe MMS Series
Technical parameters:
Coercivity: 219kA/m(2750 oe)HiCo / 28.7kA/m(360 oe LoCo
Square ratio K: ≥0.8
Base film material: Polyester film
Magnetic layer material: Barium Ferrite /
Color: Black
Base film thickness:(12±1)µm
Total thickness:(26~29)µm
Signal Amplitude Characteristics:
Signal amplitude UA1:80~130% UR
Signal amplitude Ui1:≤136% UR
Signal amplitude UA2:≥80% UR
Signal amplitude Ui2:≥65% UA2
Resolution UA3:≥70% UA2
Erasure UA4:≤3% UR
Extra pulse Ui4:≤5%
Wear Resistance Characteristics:
Average signal output amplitude: UA after≥60% UA before
Individual signal output amplitude:Ui after≥80% Ui before
Durability:≥2000 times
Chemical Resistance Characteristics:
Average signal output amplitude: UA after≥90% UA before
Individual signal output amplitude: Ui after≥90% Ui before
Storage Condition:
The allowed storage period for the magnetic stripe reel is 3 years at temperature 10~
Keep the magnetic stripe reel far away from the magnetic field.
Handle with care and avoid fierce vibration;
Keep it unexposed to sun and rain.